Skip to main content
Communities & Collections
All of IITD
Statistics
English
العربية
বাংলা
Català
Čeština
Deutsch
Ελληνικά
Español
Suomi
Français
Gàidhlig
हिंदी
Magyar
Italiano
Қазақ
Latviešu
Nederlands
Polski
Português
Português do Brasil
Srpski (lat)
Српски
Svenska
Türkçe
Yкраї́нська
Tiếng Việt
Log In
Log in
New user? Click here to register.
Have you forgotten your password?
Home
Electronic Theses and Dissertations
Electronic Theses and Dissertations
Permanent URI for this community
http://10.17.50.146:4000/handle/123456789/1
Browse
Search
Subcommunities and Collections
By Issue Date
By Author
By Title
By Subject
By Subject Category
Search
Subcommunities and Collections
By Issue Date
By Author
By Title
By Subject
By Subject Category
1 results
Back to results
Filters
Author
1
search.filters.author.Sharma, Hemant Kumar
Subject
search.filters.subject.Cyclic nanoindentation
1
search.filters.subject.Berkovich indenter
1
search.filters.subject.Cathodoluminescence
1
search.filters.subject.Pressure assisted phase transformation
1
search.filters.subject.Spherical indenter
Search subject
Submit
Browse subject tree
Date
Start
End
Submit
2023
1
Has files
Yes
Reset filters
Settings
Sort By
Accessioned Date Descending
Most Relevant
Title Ascending
Date Issued Descending
Results per page
1
5
10
20
40
60
80
100
Search
Has files: Yes
×
Subject: search.filters.subject.Cyclic nanoindentation
×
Search Tools
Search Results
Now showing
1 - 1 of 1
No Thumbnail Available
Item
Nanoindentation studies of HgCdTe epitaxial films and CdZnTe single crystal substrates
(
IIT Delhi
,
2023-02-01
)
Sharma, Hemant Kumar
Show more